Analyze the method of preparing metal carved plates for you

Your current location: Home >> News >> Company News

Analyze the method of preparing metal carved plates for you

Release date:2016-07-27 Author: Click:


内墙金属雕花板

 

    (1) Take the magnesium chloride with a relative density greater than 1.2096 into a large cylinder, stir evenly with cold water and dissolve it fully, and pour out the floating foam to obtain the raw material with a relative density of 1.209 6 for use.

    (2) Take magnesium oxide and talc powder over 60 mesh sieves, place them in a container, gradually add chlorine solution, and stir into a paste fabric for use.

    (3) Take the magnesium mesh and talcum powder of 60 mesh sieve, put the wood powder of the 10 mesh sieve into the container, add the solution and mix the 107 glue evenly, make it easy to wipe, and use it as the main material.

    (4) Spread the mold embossment up on the glass of the workbench, evenly brush the fabric on the mold, lay the first layer of glass cloth, and use the plate to loosely press the first layer of Bray cloth on the plate. On the surface, then the main material is placed on the surface of the board to be smoothed, and then the second layer of Borre cloth is placed and pressed on the main material. When the air temperature is 25 ° C, it can be turned over 24 hours.

    Evenly brush the fine fabric on the mold with the concave upwards. When the groove is full, the fabric is evenly brushed on the surface of the board. The first layer of glass cloth is placed, and the glass cloth and the surface are covered with a brush. The fabric is fully contacted, and the iron frame with iron wire is placed flat on the glass cloth, and then the main material is placed, leveled with a pressure plate, and then flattened with a square trowel to make the thickness uniform, and removed. Iron frame, put a second layer of glass cloth, flatten it with a pressure plate, put the fabric on the plate with a pressure plate, and then put a third layer of glass cloth, smooth with a pressure plate to make the fabric and glass cloth stick, the air temperature is At 25 ° C, it can be used for 24 h. After drying for 3-5 d, it can be sprayed and dried.

     Metal engraving board raw materials compatibility The content ratio of each component of the product is: magnesium oxide 3.0-3.3, talcum powder 1.2-1. 5, magnesium grabbing 3.5^-4.0, wood powder 1. 0-1. 4, 107 glue 0.2 -0.3, Boris cloth 0.3-0.4o product application This product is a building decoration material, which can be used for indoor wall decoration. How to use: Fix the wooden strip on the wall and use a rubber brush on the composite carved decorative board and the wooden strip. When the glue is slightly dry, the decorative board and the wooden strip can be compacted. Product characteristics This product has a wide range of raw materials, low cost, scientific concept, reasonable process; beautiful decoration, good effect, fireproof and moisture proof, no deformation, long service life.